Static Creep Tester
Model : CR-1300 Series
The Static Creep Tester gives a tensile or compressive constant load to a test piece in a thermostat chamber and measures the creep that changes with the time elapsed at that time.The creep can be measured at increments of 0.1mm with a rotary encoder,and maximum loads up to 1kN can be loaded.The thermostat chamber can be controlled between room temperatures +10 to 150℃,while the interval for data collection can be set to 0.5 seconds as the shortest setting.Machine operation,test condition setting,data processing,and graph plotting are performed by special designed software.
Applicable Standard:JIS K7115/JIS K7116/ ISO899
Maximum Load:100N(Option:1kN)
Maximum Stroke:70mm
Test temperature:RT+10~150℃(Low temperature is possible by option)